LNP™ STAT-KON™ Compound DX13315C

Want to keep this datasheet? Save it now in your required format

Description

LNPTM Stat-KonTM DX13315C is an electrical conductive thermoplastic compound featuring electrostatic discharge (ESD) safe performance based on a unique Ultra Clean Polycarbonate (PC) resin reinforced with 15% carbon fiber. This compound provides good stiffness, dimension stability and has extremely high level of cleanliness for the most demanding applications in the Hard Disk Drive and Semiconductor industry. A unique feature of this material is its low C18-C40 hydrocarbons and this compound is manufactured using the LNP Clean Compounding Solution (CCS) technology.

Los datos sobre este material han sido proporcionados por Sabic.

A menos que se indique lo contrario, todas las medidas corresponden a condiciones de temperatura ambiente. A menos que se indique lo contrario, se utilizan las unidades del SI.
Las normas armonizadas son similares a uno o varios estándares del proveedor. Es posible que algunas normas armonizadas se ajusten al estándar original, mientras que otras pueden quedar fuera de su alcance.

Ashby charts

Propiedades

General

PropertyTemperatureValueComment

Densidad relativa

23.0 °C

1.26 [-]

Show Supplier Material materials with Densidad relativa of 1.26 [-]

ASTM D 792 |

Mecánica

PropertyTemperatureValueComment

Elongación

23.0 °C

2.6 %

Show Supplier Material materials with Elongación of 2.6 %

ISO 527 | break, 5 mm/min

Impact strength, Izod notched, ASTM

23.0 °C

88 J/m

Show Supplier Material materials with Impact strength, Izod notched, ASTM of 88 J/m

ASTM D 256 | notched, 23°C

Impact strength, Izod unnotched, ASTM

23.0 °C

591 J/m

Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 591 J/m

ASTM D 4812 | 23°C

Módulo de flexión

23.0 °C

9.3 GPa

Show Supplier Material materials with Módulo de flexión of 9.3 GPa

ISO 178 | 2 mm/min

Módulo elástico

23.0 °C

10.6 GPa

Show Supplier Material materials with Módulo elástico of 10.6 GPa

ISO 527 | 1 mm/min

Resistencia a la flexión

23.0 °C

203 MPa

Show Supplier Material materials with Resistencia a la flexión of 203 MPa

ISO 178 | yield, 2 mm/min

Resistencia a la tracción

23.0 °C

130 MPa

Show Supplier Material materials with Resistencia a la tracción of 130 MPa

ISO 527 | break, 5 mm/min

Resistencia al choque, ensayo Charpy entallado

23.0 °C

9 kJ/m²

Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 9 kJ/m²

ISO 179/2C | 23°C

Resistencia al choque, ensayo Charpy no entallado

23.0 °C

45 kJ/m²

Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 45 kJ/m²

ISO 179/2C | 23°C

Resistencia al choque, ensayo Izod entallado

23.0 °C

88 kJ/m²

Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 88 kJ/m²

ASTM D 256 | notched, 23°C

Aplicaciones térmicas

PropertyTemperatureValueComment

Coeficiente de dilatación térmica

23.0 °C

1.4E-5 1/K

Show Supplier Material materials with Coeficiente de dilatación térmica of 1.4E-5 1/K

ASTM E 831 | -40°C to 40°C

Coeficiente de dilatación térmica transversal

23.0 °C

8.1E-5 1/K

Show Supplier Material materials with Coeficiente de dilatación térmica transversal of 8.1E-5 1/K

ASTM E 831 | -40°C to 40°C

Heat deflection temperature, 1.80 MPa

123 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 123 °C

ASTM D 648 | 3.2mm, unannealed

Temperatura de flexión bajo carga

123 °C

Show Supplier Material materials with Temperatura de flexión bajo carga of 123 °C

Inflamabilidad

UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=102010749- - <br> UL Recognized, 94HB Flame Class Rating: 1mm UL 94

Eléctrico

PropertyTemperatureValueComment

Sheet resistivity, ROA

23.0 °C

5000 - 500000 Ω

Show Supplier Material materials with Sheet resistivity, ROA of 5000 - 500000 Ω

ASTM D 257

Volume resistivity

23.0 °C

5.00E+4 - 5.00E+6 Ω·cm

Show Supplier Material materials with Volume resistivity of 5.00E+4 - 5.00E+6 Ω·cm

ASTM D 257

Rheological Properties

PropertyTemperatureValueComment

Contracción

23.0 °C

0.1 %

Show Supplier Material materials with Contracción of 0.1 %

SABIC method | 3.2 mm

Contracción transversal

23.0 °C

0.2 %

Show Supplier Material materials with Contracción transversal of 0.2 %

SABIC method | 3.2 mm

Velocidad de flujo del volumen derretido

30 cm³/10min

Show Supplier Material materials with Velocidad de flujo del volumen derretido of 30 cm³/10min

ISO 1133 | MVR at 300°C/5.0 kg

Technological properties

Property
Availability

Europe,Asia,Americas

Processing methods

Drying Temperature: 90 to 110.0°C
Drying Time: 3 to 5.0hrs
Melt Temperature: 280 to 320.0°C
Nozzle Temperature: 280 to 320.0°C
Front - Zone 3 Temperature: 280 to 320.0°C
Middle - Zone 2 Temperature: 280 to 320.0°C
Rear - Zone 1 Temperature: 250 to 280.0°C
Mold Temperature: 90 to 120.0°C
Back Pressure: 1 to 5.0MPa
Screw Speed: 30 to 100.0rpm

Supplier Disclaimer

While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right.