Heat deflection temperature, 1.80 MPa: 123 °C

Quick Comparison

Policarbonato (PC)

LEXAN™ FR Resins LUX9612G

Policarbonato (PC)

LEXAN™ Resin LUX2114G

Policarbonato (PC)

LEXAN™ Resin LUX2614G

Polyvinylidenefluoride (PVDF)

Kynar® 370

Suministrada por:

Arkema: High Performance Polymers

Policarbonato (PC)

LEXAN™ Copolymer EXL8454 - Asia

Suministrada por:

Sabic

Policarbonato (PC)

LEXAN™ Copolymer EXL8454 - Europe

Suministrada por:

Sabic

Policarbonato (PC)

LEXAN™ Copolymer EXL8483 - Asia

Suministrada por:

Sabic

Policarbonato (PC)

LEXAN™ Copolymer EXL8483 - Europe

Suministrada por:

Sabic

Policarbonato (PC)

LEXAN™ Copolymer EXL8134 - Asia

Suministrada por:

Sabic

Policarbonato (PC)

LEXAN™ Copolymer EXL8134 - Europe

Suministrada por:

Sabic

Éter de polifenileno (PPE)

NORYL™ Resin LTA6020 - Europe

Suministrada por:

Sabic

Éter de polifenileno (PPE)

NORYL™ Resin LTA6020 - Asia

Suministrada por:

Sabic

Éter de polifenileno (PPE)

NORYL™ Resin LTA6020 - Americas

Suministrada por:

Sabic

Éter de polifenileno (PPE)

NORYL™ Resin EN265 - Americas

Suministrada por:

Sabic

Policarbonato (PC)

LEXAN™ Copolymer FXE4472L - Asia

Suministrada por:

Sabic

Policarbonato (PC)

LNP™ STAT-KON™ Compound DX13315C

Suministrada por:

Sabic

Mezcla de polímeros

CYCOLOY™ FR Resins C4210HF

Tereftalato de polibutileno (PBT)

LNP™ FARADEX™ Compound WX94736

Suministrada por:

Sabic

Policarbonato (PC)

LNP™ LUBRICOMP™ Compound DX98306H - Asia

Suministrada por:

Sabic

Policarbonato (PC)

LNP™ LUBRICOMP™ Compound DX98306H - Americas

Suministrada por:

Sabic
Página 1 de 2