General
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of friction | 0.33 - 0.47 [-] Show Supplier Material materials with Coefficient of friction of 0.33 - 0.47 [-] | ||
Coefficient of friction, kinetic | 0.47 [-] Show Supplier Material materials with Coefficient of friction, kinetic of 0.47 [-] | ASTM D 3702 Modified: Manual | |
Coefficient of friction, static | 0.33 [-] Show Supplier Material materials with Coefficient of friction, static of 0.33 [-] | ASTM D 3702 Modified: Manual | |
Densidad | 23.0 °C | 1.51 g/cm³ Show Supplier Material materials with Densidad of 1.51 g/cm³ | ASTM D 792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 1.6 % Show Supplier Material materials with Elongación of 1.6 % | ASTM D 638 | break |
Impact strength, Izod notched, ASTM | 23.0 °C | 55 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 55 J/m | ASTM D 256 |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 485 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 485 J/m | ASTM D 4812 | 23°C |
Módulo de flexión | 23.0 °C | 19.9 GPa Show Supplier Material materials with Módulo de flexión of 19.9 GPa | ASTM D 790 |
Módulo elástico | 23.0 °C | 18.1 GPa Show Supplier Material materials with Módulo elástico of 18.1 GPa | ASTM D 638 | 50 mm/min |
Resistencia a la flexión | 23.0 °C | 245 MPa Show Supplier Material materials with Resistencia a la flexión of 245 MPa | ASTM D 790 |
Resistencia a la tracción | 23.0 °C | 157 MPa Show Supplier Material materials with Resistencia a la tracción of 157 MPa | ASTM D 638 | break |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 55 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 55 kJ/m² | ASTM D 256 | notched, 23°C |
Aplicaciones térmicas
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 10 - 100 Ω Show Supplier Material materials with Sheet resistivity, ROA of 10 - 100 Ω | ASTM D 257 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 120 to 150.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |