Copolyamide 6/66 (PA6/66)
RADILON CA RV300L 333 BKSuministrada por:
RadiciGroup High Performance PolymersPolioximetileno (POM)
Delrin® 525GR NC000Polyphenylene Sulfide (PPS)
PPS GF30 SG301R65Suministrada por:
Shandong Sciengy New Materials Co. LtdPolyphenylene Sulfide (PPS)
PPS GF60 MD SGM601E65Suministrada por:
Shandong Sciengy New Materials Co. LtdCompuesto de matriz cerámica a base de carburos
SIGRASIC® Carbon Fiber Reinforced Silicon Carbide FeltSuministrada por:
SGL Carbon