General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad relativa | 23.0 °C | 1.61 [-] Show Supplier Material materials with Densidad relativa of 1.61 [-] | ASTM D 792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 2.2 % Show Supplier Material materials with Elongación of 2.2 % | ISO 527 | break, 5 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 166 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 166 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 669 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 669 J/m | ASTM D 4812 | 23°C |
Módulo de flexión | 23.0 °C | 11.9 GPa Show Supplier Material materials with Módulo de flexión of 11.9 GPa | ISO 178 | 2 mm/min |
Módulo elástico | 23.0 °C | 14.1 GPa Show Supplier Material materials with Módulo elástico of 14.1 GPa | ISO 527 | 1 mm/min |
Resistencia a la flexión | 23.0 °C | 206 MPa Show Supplier Material materials with Resistencia a la flexión of 206 MPa | ISO 178 | break, 2 mm/min |
Resistencia a la tracción | 23.0 °C | 152 MPa Show Supplier Material materials with Resistencia a la tracción of 152 MPa | ISO 527 | break, 5 mm/min |
Resistencia al choque, ensayo Charpy entallado | 23.0 °C | 16 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 16 kJ/m² | ISO 179/2C | 23°C |
Resistencia al choque, ensayo Charpy no entallado | 23.0 °C | 43 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 43 kJ/m² | ISO 179/2C | 23°C |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 166 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 166 kJ/m² | ASTM D 256 | notched, 23°C |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 1.6E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.6E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Coeficiente de dilatación térmica transversal | 23.0 °C | 6E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica transversal of 6E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Heat deflection temperature, 0.45 MPa | 128 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 128 °C | ASTM D 648 | 3.2 mm, unannealed | |||
Relative temperature index, electrical | 80 °C Show Supplier Material materials with Relative temperature index, electrical of 80 °C | UL 746B | |||
Relative temperature index, mechanical impact | 80 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 80 °C | UL 746B | |||
Relative temperature index, mechanical strength | 80 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 80 °C | UL 746B | |||
Temperatura de flexión bajo carga | 128 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 128 °C | ||||
Inflamabilidad | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=102010576- - <br> UL Recognized, 94HB Flame Class Rating: ≥0.4mm UL 94 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.05 % Show Supplier Material materials with Contracción of 0.05 % | SABIC method | 3.2 mm |
Contracción transversal | 23.0 °C | 0.1 % Show Supplier Material materials with Contracción transversal of 0.1 % | SABIC method | 3.2 mm |
Velocidad de flujo del volumen derretido | 18 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 18 cm³/10min | ISO 1133 | MVR at 300°C/5.0 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Personal Computing, Smart/ID Card, Photo/Video Camera, Wireless Communications, Document Handling, Enclosures | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 90 to 110.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |