General
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of friction | 0.41 - 0.46 [-] Show Supplier Material materials with Coefficient of friction of 0.41 - 0.46 [-] | ||
Coefficient of friction, kinetic | 0.46 [-] Show Supplier Material materials with Coefficient of friction, kinetic of 0.46 [-] | ASTM D 3702 Modified: Manual | |
Coefficient of friction, static | 0.41 [-] Show Supplier Material materials with Coefficient of friction, static of 0.41 [-] | ASTM D 3702 Modified: Manual | |
Densidad | 23.0 °C | 1.54 g/cm³ Show Supplier Material materials with Densidad of 1.54 g/cm³ | ASTM D 792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 2.6 % Show Supplier Material materials with Elongación of 2.6 % | ISO 527 | yield |
Módulo de flexión | 23.0 °C | 8.3 GPa Show Supplier Material materials with Módulo de flexión of 8.3 GPa | ISO 178 |
Resistencia a la flexión | 23.0 °C | 185 MPa Show Supplier Material materials with Resistencia a la flexión of 185 MPa | ISO 178 |
Resistencia a la tracción | 23.0 °C | 118 MPa Show Supplier Material materials with Resistencia a la tracción of 118 MPa | ISO 527 | yield |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 16 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 16 kJ/m² | ISO 180/1A | notched 80*10*4, 23°C |
Resistencia al choque, ensayo Izod no entallado | 23.0 °C | 55 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod no entallado of 55 kJ/m² | ISO 180/1U | 80*10*4, 23°C |
Aplicaciones térmicas
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 143 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 143 °C | ASTM D 648 | 3.2mm, unannealed | |
Temperatura de flexión bajo carga | 143 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 143 °C | ||
Inflamabilidad | UL Recognized, 94V-1 Flame Class Rating: ≥3mm UL 94 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101344609- - |
Technological properties
Property | ||
---|---|---|
Application areas | Small Appliance, Photovoltaic Components, Plumbing, Medical Device, Meter Water, Personal Computing, Document Handling, Displays, Data Management, Electronic Components, Lab Ware and Clinical Diagnostics | |
Availability | Europe,Americas | |
Processing methods | Middle - Zone 2 Temperature: 310 to 320.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |