Coefficient of friction, kinetic: 0.46 [-]

Quick Comparison

Policarbonato (PC)

LNP™ LUBRICOMP™ Compound DFL34EH

Suministrada por:

Sabic

Tereftalato de polibutileno (PBT)

LNP™ LUBRICOMP™ Compound WFL33

Suministrada por:

Sabic

Acrilonitrilo butadieno estireno (ABS)

LNP™ LUBRICOMP™ Compound AI001XXH

Suministrada por:

Sabic

Polyamide 66 (PA66)

LNP™ LUBRICOMP™ Compound RX03643H

Suministrada por:

Sabic

Polyamide 610 (PA610)

LNP™ LUBRICOMP™ Compound QCP36

Suministrada por:

Sabic

Polyamide 612 (PA612)

LNP™ LUBRICOMP™ Compound IFL34

Suministrada por:

Sabic

Policarbonato (PC)

LNP™ LUBRICOMP™ Compound DX00714H

Suministrada por:

Sabic

Poliftalamida (PPA)

LNP™ LUBRICOMP™ Compound UFL36S - Asia

Suministrada por:

Sabic

Polietersulfona (PES)

LNP™ LUBRICOMP™ Compound JFL36 - Americas

Suministrada por:

Sabic

Polietersulfona (PES)

LNP™ LUBRICOMP™ Compound JFL36 - Asia

Suministrada por:

Sabic

Polietersulfona (PES)

LNP™ LUBRICOMP™ Compound JFL36 - Europe

Suministrada por:

Sabic

Polyamide 612 (PA612)

LNP™ LUBRICOMP™ Compound IFL36 - Americas

Suministrada por:

Sabic

Policarbonato (PC)

LNP™ LUBRICOMP™ Compound DFL36 - Americas

Suministrada por:

Sabic

Policarbonato (PC)

LNP™ LUBRICOMP™ Compound DFL36 - Europe

Suministrada por:

Sabic