General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 0.07 % Show Supplier Material materials with Absorción de agua of 0.07 % | ASTM D 570 | (23°C/24hrs) |
Densidad relativa | 23.0 °C | 1.08 [-] Show Supplier Material materials with Densidad relativa of 1.08 [-] | ASTM D 792 |
Índice límite de óxigeno | 23.0 °C | 29.2 % Show Supplier Material materials with Índice límite de óxigeno of 29.2 % |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 25 % Show Supplier Material materials with Elongación of 25 % | ASTM D 638 | brk, Type I, 50 mm/min |
Gardner Impact | 23.0 °C | 4 J Show Supplier Material materials with Gardner Impact of 4 J | ASTM D 3029 | -40°C |
Hardness, Rockwell R | 23.0 °C | 119 [-] Show Supplier Material materials with Hardness, Rockwell R of 119 [-] | ASTM D 785 |
Impact strength, Izod notched, ASTM | 23.0 °C | 186 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 186 J/m | ASTM D 256 |
Módulo de flexión | 23.0 °C | 2.6 GPa Show Supplier Material materials with Módulo de flexión of 2.6 GPa | ASTM D 790 | 2.6 mm/min, 100 mm span |
Resistencia a la flexión | 23.0 °C | 99 MPa Show Supplier Material materials with Resistencia a la flexión of 99 MPa | ASTM D 790 | yld, 2.6 mm/min, 100 mm span |
Resistencia a la tracción | 23.0 °C | 63 MPa Show Supplier Material materials with Resistencia a la tracción of 63 MPa | ASTM D 638 | yld, Type I, 50 mm/min |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 186 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 186 kJ/m² | ASTM D 256 | notched, 23°C |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 5.94E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 5.94E-5 1/K | ASTM E 831 | -40°C to 95°C | ||
Glow Wire Flammability Index | 960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | ||||
Glow Wire Ignition Temperature | 725 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 725 °C | IEC 60695-2-13 | 2.0 mm | |||
Heat deflection temperature, 1.80 MPa | 123 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 123 °C | ASTM D 648 | 6.4 mm, unannealed | |||
Relative temperature index, electrical | 110 °C Show Supplier Material materials with Relative temperature index, electrical of 110 °C | UL 746B | |||
Relative temperature index, mechanical impact | 105 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 105 °C | UL 746B | |||
Relative temperature index, mechanical strength | 110 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 110 °C | UL 746B | |||
Temperatura de flexión bajo carga | 123 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 123 °C | ||||
Inflamabilidad | UL Recognized, 94V-1 Flame Class Rating: ≥1.5mm UL 94 <br> UL Recognized, 94V-0 Flame Class Rating: ≥6mm UL 94 <br> UV-light, water exposure/immersion: F1- UL 746C <br> Radiant Panel Listing: RP100- UL Tested <br> Glow Wire Flammability Index, 1.0 mm: 900°C IEC 60695-2-12 <br> Glow Wire Flammability Index, 1.5 mm: 900°C IEC 60695-2-12 <br> Glow Wire Ignitability Temperature, 1.0 mm: 700°C IEC 60695-2-13 <br> Glow Wire Ignitability Temperature, 1.5 mm: 700°C IEC 60695-2-13 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=221239- - |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Dielectric constant, 60Hz | 23.0 °C | 2.69 [-] Show Supplier Material materials with Dielectric constant, 60Hz of 2.69 [-] | ASTM D 150 | 50/60 Hz |
Dissipation factor, 50Hz | 23.0 °C | 7E-4 [-] Show Supplier Material materials with Dissipation factor, 50Hz of 7E-4 [-] | ASTM D 150 | 50/60 Hz |
High Amp Arc Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with High Amp Arc Ignition of 1.5 mm | ≥, UL 746A | PLC 0 |
High Volt Arc Track Rate | 23.0 °C | 4 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 4 PLC Code | UL 746A | (PLC) |
Hot-Wire Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with Hot-Wire Ignition of 1.5 mm | ≥, UL 746A | PLC 0 |
Rigidez dieléctrica | 23.0 °C | 19.6 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 19.6 kV/mm | ASTM D 149 | in oil, 3.2 mm |
Índice de seguimiento comparativo | 23.0 °C | 1 V Show Supplier Material materials with Índice de seguimiento comparativo of 1 V | UL 746A | (UL) {PLC} |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.5 % Show Supplier Material materials with Contracción of 0.5 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Power Boat, Photovoltaic Components, Pharmaceutical Packaging & Drug Delivery, Building/Construction Sheet, Circuit Protection, Electronic Components, Enclosure/Housing/Cover, Heavy Vehicles | |
Availability | Americas | |
Processing methods | Melt Temperature: 225 to 255.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |