General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Supplier Material materials with Densidad of 7.8 g/cm³ | typical for steels |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Brinell | 23.0 °C | 215 [-] Show Supplier Material materials with Dureza Brinell of 215 [-] | |
Elongación A5 | 23.0 °C | 35 - 45 % Show Supplier Material materials with Elongación A5 of 35 - 45 % | |
Límite elástico Rp 0,2 | 23.0 °C | 180 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 180 MPa | |
Módulo elástico | 23.0 °C | 200 - 210 GPa Show Supplier Material materials with Módulo elástico of 200 - 210 GPa | typical for steels |
Resistencia a la tracción | 23.0 °C | 460 - 680 MPa Show Supplier Material materials with Resistencia a la tracción of 460 - 680 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.03 % Show Supplier Material materials with Azufre of 0.03 % |
Carbono | 0.03 % Show Supplier Material materials with Carbono of 0.03 % |
Cromo | 18 - 20 % Show Supplier Material materials with Cromo of 18 - 20 % |
Fósforo | 0.05 % Show Supplier Material materials with Fósforo of 0.05 % |
Manganeso | 2 % Show Supplier Material materials with Manganeso of 2 % |
Nitrógeno | 0.1 % Show Supplier Material materials with Nitrógeno of 0.1 % |
Níquel | 8 - 12 % Show Supplier Material materials with Níquel of 8 - 12 % |
Silicona | 0.75 % Show Supplier Material materials with Silicona of 0.75 % |