EN 1.4306

Quick Comparison

Acero inoxidable austenítico

Sandvik 3R12

Suministrada por:

Alleima (formerly Sandvik Materials Technology)

Acero inoxidable austenítico

DIN 17440 Grade X2CrNi19-11 quenched (+Q)

Acero inoxidable austenítico

DIN 1654-5 Grade X2CrNi19-11 quenched (+Q)

Acero inoxidable austenítico

JIS G4303 Grade SUS304L solution treated

Acero inoxidable austenítico

JIS G4304 Grade SUS304L solution treated

Acero inoxidable austenítico

JIS G4305 Grade SUS304L solution treated

Acero inoxidable austenítico

JIS G3459 Grade SUS304LTP

Acero inoxidable austenítico

JIS G3468 Grade SUS304LTPY

Acero inoxidable austenítico

JIS G3463 Grade SUS304LTB