General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8 g/cm³ Show Supplier Material materials with Densidad of 8 g/cm³ |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminio | 0.15 - 0.6 % Show Supplier Material materials with Aluminio of 0.15 - 0.6 % | |
Carbono | 0.06 - 0.1 % Show Supplier Material materials with Carbono of 0.06 - 0.1 % | |
Cobre | 0.75 % Show Supplier Material materials with Cobre of 0.75 % | |
Cromo | 19 - 23 % Show Supplier Material materials with Cromo of 19 - 23 % | |
Hierro | 39.5 % Show Supplier Material materials with Hierro of 39.5 % | min. |
Manganeso | 1.5 % Show Supplier Material materials with Manganeso of 1.5 % | max. |
Níquel | 30 - 35 % Show Supplier Material materials with Níquel of 30 - 35 % | |
Silicona | 1 % Show Supplier Material materials with Silicona of 1 % | max. |
Titanio | 0.15 - 0.6 % Show Supplier Material materials with Titanio of 0.15 - 0.6 % |