General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 0.02 % Show Supplier Material materials with Absorción de agua of 0.02 % | ISO 62 |
Densidad | 23.0 °C | 1.57 g/cm³ Show Supplier Material materials with Densidad of 1.57 g/cm³ | ISO 1183 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 1.9 % Show Supplier Material materials with Elongación of 1.9 % | ISO 527 |
Módulo de flexión | 23.0 °C | 11 GPa Show Supplier Material materials with Módulo de flexión of 11 GPa | ISO 178 |
Resistencia a la flexión | 23.0 °C | 250 MPa Show Supplier Material materials with Resistencia a la flexión of 250 MPa | ISO 178 |
Resistencia a la tracción | 23.0 °C | 160 MPa Show Supplier Material materials with Resistencia a la tracción of 160 MPa | ISO 527 |
Resistencia al choque, ensayo Charpy entallado | 23.0 °C | 11 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 11 kJ/m² | ISO 179 |
Aplicaciones térmicas
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 260 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 260 °C | ISO 75 | |
Temperatura de fusión | 280 °C Show Supplier Material materials with Temperatura de fusión of 280 °C | ISO 11357 (10°C/min) | |
Temperatura máx. de funcionamiento | 260 °C Show Supplier Material materials with Temperatura máx. de funcionamiento of 260 °C | ||
Inflamabilidad | V-0, UL-94 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Constante dieléctrica | 23.0 °C | 4 [-] Show Supplier Material materials with Constante dieléctrica of 4 [-] | IEC 60250 |
Factor de disipación | 23.0 °C | 2E-3 [-] Show Supplier Material materials with Factor de disipación of 2E-3 [-] | IEC 60250 |
Rigidez dieléctrica | 23.0 °C | 16 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 16 kV/mm | IEC 60243 |
Volume resistivity | 23.0 °C | 2.40E+15 Ω·cm Show Supplier Material materials with Volume resistivity of 2.40E+15 Ω·cm | IEC 60093 |
Índice de seguimiento comparativo | 23.0 °C | 125 V Show Supplier Material materials with Índice de seguimiento comparativo of 125 V | IEC 60112 |
Technological properties
Property | ||
---|---|---|
Application areas | In the electronics industry for the production of connectors, wiring device, frequency divider and a variety of instrument components, such as shell; in the aerospace industry for the production of high strength, high temperature resistant and insulation of the high performance requirements of thin-walled parts; in the chemical industry for the production of corrosion-resistant valves, insulation devices in military products, for the production of precision electrical connectors, high strength, high temperature resistant contactor shell, motor module, pump impeller, pump, chemical pump etc. | |
Fillers | 30% Glass Fiber | |
Processing methods | Injection Moulding / Test Specimen Production: Drying: 150°C & 3 hours - Injection Pressure: 30-100 MPa - Injection Molding Melt Temperature: 290-330°C - Injection Molding Mold Temperature: 120-160°C - Limit in-cylinder Retention Time: 300°C/60min or 320°C/30min |