General
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 1.2 % Show Supplier Material materials with Elongación of 1.2 % | ISO 527 |
Módulo de flexión | 23.0 °C | 14 GPa Show Supplier Material materials with Módulo de flexión of 14 GPa | ISO 178 |
Resistencia a la flexión | 23.0 °C | 200 MPa Show Supplier Material materials with Resistencia a la flexión of 200 MPa | ISO 178 |
Resistencia a la tracción | 23.0 °C | 125 MPa Show Supplier Material materials with Resistencia a la tracción of 125 MPa | ISO 527 |
Resistencia al choque, ensayo Charpy entallado | 23.0 °C | 6.5 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 6.5 kJ/m² | ISO 179 |
Aplicaciones térmicas
Technological properties
Property | ||
---|---|---|
Application areas | Can be used in the production of gear, bearing, slide and low friction coefficient, low friction consumption | |
Fillers | 10% Carbon Fiber | |
Processing methods | Injection Moulding / Test Specimen Production: Drying: 150°C & 3 hours - Injection Pressure: 30-100 MPa - Injection Molding Melt Temperature: 290-330°C - Injection Molding Mold Temperature: 120-160°C - Limit in-cylinder Retention Time: 300°C/60min or 320°C/30min |