Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 80 % Show Supplier Material materials with Elongación of 80 % | ISO 527 |
Módulo de flexión | 23.0 °C | 1.5 GPa Show Supplier Material materials with Módulo de flexión of 1.5 GPa | ISO 178 |
Resistencia a la flexión | 23.0 °C | 60 MPa Show Supplier Material materials with Resistencia a la flexión of 60 MPa | ISO 178 |
Resistencia a la tracción | 23.0 °C | 40 MPa Show Supplier Material materials with Resistencia a la tracción of 40 MPa | ISO 527 |
Resistencia al choque, ensayo Charpy entallado | 23.0 °C | 30 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 30 kJ/m² | ISO 179 |
Aplicaciones térmicas
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 90 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 90 °C | ISO 75 | |
Inflamabilidad | V-1, UL94 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Constante dieléctrica | 23.0 °C | 3 [-] Show Supplier Material materials with Constante dieléctrica of 3 [-] | IEC 60250 |
Factor de disipación | 23.0 °C | 2E-3 [-] Show Supplier Material materials with Factor de disipación of 2E-3 [-] | IEC 60250 |
Rigidez dieléctrica | 23.0 °C | 24 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 24 kV/mm | IEC 60243 |
Technological properties
Property | ||
---|---|---|
Application areas | This extrusion grade is in automobile pipeline, sunroof, water pipe, intermediate cooling pipe, radiator vent pipe, cooling pipe, fuel filler pipe, fuel tank fuel supply pipe, transmission vent pipe, crankcase ventilation pipe, turbocharger pipe, etc., ocean Pipes, chemical fields, oil pipelines and other fields have a wide range of applications. | |
Processing methods | Extrusion or Injection Moulding / Test Specimen Production: Drying 80°C & 5 hours - Hopper Temperature: 20-40°C - Extruder Zone Temperature: 300-320°C - Adaptor Temperature: 290-310°C - Die Temperature: 300-320°C - Melt Temperature: 315-320°C |