General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.4 g/cm³ Show Supplier Material materials with Densidad of 1.4 g/cm³ | ISO 1183 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 25 % Show Supplier Material materials with Elongación of 25 % | ISO 527 |
Módulo de flexión | 23.0 °C | 3.2 GPa Show Supplier Material materials with Módulo de flexión of 3.2 GPa | ISO 178 |
Resistencia a la flexión | 23.0 °C | 100 MPa Show Supplier Material materials with Resistencia a la flexión of 100 MPa | ISO 178 |
Resistencia a la tracción | 23.0 °C | 80 MPa Show Supplier Material materials with Resistencia a la tracción of 80 MPa | ISO 527 |
Resistencia al choque, ensayo Charpy entallado | 23.0 °C | 7.5 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 7.5 kJ/m² | ISO 179 |
Aplicaciones térmicas
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Constante dieléctrica | 23.0 °C | 2.8 [-] Show Supplier Material materials with Constante dieléctrica of 2.8 [-] | IEC 60250 |
Factor de disipación | 23.0 °C | 4E-3 [-] Show Supplier Material materials with Factor de disipación of 4E-3 [-] | IEC 60250 |
Rigidez dieléctrica | 23.0 °C | 26 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 26 kV/mm | IEC 60243 |
Volume resistivity | 23.0 °C | 1.00E+16 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+16 Ω·cm | IEC 60093 |
Índice de seguimiento comparativo | 23.0 °C | 150 V Show Supplier Material materials with Índice de seguimiento comparativo of 150 V | IEC 60112 |
Technological properties
Property | ||
---|---|---|
Application areas | Chemical pump pump body and impeller, cable plug, junction box, ultra pure water system pipe fittings and valves.Engine bearing, shim, sealing element, clutch ring.The driving and brake parts of a car. Cable, wire, coil skeleton, connector, etc | |
Processing methods | Extrusion or Injection Moulding / Test Specimen Production: Drying 150°C & 3 hours/120°C & 5 hours - Injection molding melt temperature: 355-375°C - Injection molding mold temperature: 170-200°C |