General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 0.04 % Show Supplier Material materials with Absorción de agua of 0.04 % | ISO 62 |
Densidad | 23.0 °C | 1.45 g/cm³ Show Supplier Material materials with Densidad of 1.45 g/cm³ | ISO 1183 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 2.2 % Show Supplier Material materials with Elongación of 2.2 % | ISO 527 |
Módulo de flexión | 23.0 °C | 11 GPa Show Supplier Material materials with Módulo de flexión of 11 GPa | ISO 178 |
Resistencia a la flexión | 23.0 °C | 230 MPa Show Supplier Material materials with Resistencia a la flexión of 230 MPa | ISO 178 |
Resistencia a la tracción | 23.0 °C | 150 MPa Show Supplier Material materials with Resistencia a la tracción of 150 MPa | ISO 527 |
Resistencia al choque, ensayo Charpy entallado | 23.0 °C | 8 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 8 kJ/m² | ISO 179 |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Conductividad térmica | 23.0 °C | 0.8 W/(m·K) Show Supplier Material materials with Conductividad térmica of 0.8 W/(m·K) | ISO 22007-4 | ||
Heat deflection temperature, 1.80 MPa | 315 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 315 °C | ISO 75 | |||
Temperatura de fusión | 343 °C Show Supplier Material materials with Temperatura de fusión of 343 °C | ISO 11357 (10°C/min) | |||
Inflamabilidad | V-0, UL-94 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Volume resistivity | 23.0 °C | 1.00E+10 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+10 Ω·cm | IEC 60093 |
Technological properties
Property | ||
---|---|---|
Application areas | Chemical pump pump body and impeller, cable plug, junction box, ultra pure water system pipe fittings and valves.Engine bearing, shim, sealing element, clutch ring.The driving and brake parts of a car. Cable, wire, coil skeleton, connector, etc | |
Fillers | 30% Carbon Fiber and PTFE | |
Processing methods | Extrusion or Injection Moulding / Test Specimen Production: Drying 150°C & 3 hours/120°C & 5 hours - Injection molding melt temperature: 360-385°C - Injection molding mold temperature: 180-200°C |