General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.39 g/cm³ Show Supplier Material materials with Densidad of 1.39 g/cm³ | ISO1183 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Rockwell M | 23.0 °C | 95 [-] Show Supplier Material materials with Dureza Rockwell M of 95 [-] | ISO 2039 |
Elongación | 23.0 °C | 6 % Show Supplier Material materials with Elongación of 6 % | ISO527 |
Hardness, Rockwell L | 23.0 °C | 106 [-] Show Supplier Material materials with Hardness, Rockwell L of 106 [-] | ISO 2039 |
Hardness, Rockwell R | 23.0 °C | 115 [-] Show Supplier Material materials with Hardness, Rockwell R of 115 [-] | ISO 2039 |
Módulo de flexión | 23.0 °C | 8.5 GPa Show Supplier Material materials with Módulo de flexión of 8.5 GPa | ISO178 |
Resistencia a la flexión | 23.0 °C | 275 MPa Show Supplier Material materials with Resistencia a la flexión of 275 MPa | ISO178 |
Resistencia a la tracción | 23.0 °C | 185 MPa Show Supplier Material materials with Resistencia a la tracción of 185 MPa | ISO527 |
Resistencia al choque, ensayo Charpy entallado | 23.0 °C | 12 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 12 kJ/m² | ISO179 |
Resistencia al choque, ensayo Charpy no entallado | 23.0 °C | 70 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 70 kJ/m² | ISO179 |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Heat deflection temperature, 1.80 MPa | 254 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 254 °C | ISO 75/A |
Temperatura de fusión | 265 - 270 °C Show Supplier Material materials with Temperatura de fusión of 265 - 270 °C | ISO3146 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Volume resistivity | 23.0 °C | 1.00E+17 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+17 Ω·cm | GB/T1410 |
Rheological Properties
Property | Value | Comment |
---|---|---|
Velocidad de flujo de la masa derretida | 23 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 23 g/10min | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Application areas | Automotive industry, machinery shields, military products, building materials, etc. | |
Fillers | 33% Glass Fiber |