Heat deflection temperature, 1.80 MPa: 254 °C

Quick Comparison

Polyamide 6T (PA6T)

Zytel® HTN51G15HSL NC010

Polyamide 66 (PA66)

Zytel® LM70G35HSLX BK314

Polyamide 66 (PA66)

Zytel® PLS95G50DH2 BK261

Poliftalamida (PPA)

LNP™ LUBRICOMP™ Compound UX06425

Suministrada por:

Sabic

Polyamide 66 (PA66)

LNP™ THERMOCOMP™ Compound RF00CSXZ

Suministrada por:

Sabic

Polyamide 66 (PA66)

PA66 L2730G

Suministrada por:

HENAN SHENMA HUAWEI PLASTIC CO.,LTD.

Polyamide 66 (PA66)

LNP™ THERMOCOMP™ Compound RC00A

Suministrada por:

Sabic

Polyamide 66 (PA66)

LNP™ STAT-KON™ Compound RE006 - Americas

Suministrada por:

Sabic

Polyamide 66 (PA66)

LNP™ THERMOCOMP™ Compound RF00CSXS - Europe

Suministrada por:

Sabic

Polyamide 66 (PA66)

LNP™ THERMOCOMP™ Compound RF00C - Americas

Suministrada por:

Sabic

Polyamide 66 (PA66)

LNP™ THERMOCOMP™ Compound RF00C - Europe

Suministrada por:

Sabic

Polyamide 66 (PA66)

LNP™ LUBRICOMP™ Compound RFN18SXS

Suministrada por:

Sabic

Polyamide 66 (PA66)

LNP™ THERMOCOMP™ Compound RF009H

Suministrada por:

Sabic