General
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 120.0 °C | 4 - 5 % Show Supplier Material materials with Contracción of 4 - 5 % | GOST 18616, ISO 11501, ASTM D1204 (Thermal shrinkage at 120˚C, 5 min) |
Contracción transversal | 120.0 °C | 2 - 3 % Show Supplier Material materials with Contracción transversal of 2 - 3 % | GOST 18616, ISO 11501, ASTM D1204 (Thermal shrinkage at 120˚C, 5 min) |
Densidad | 20.0 °C | 0.91 g/cm³ Show Supplier Material materials with Densidad of 0.91 g/cm³ | |
Densidad superficial | 20.0 °C | 1.36E-3 - 4.37E-3 g/cm² Show Supplier Material materials with Densidad superficial of 1.36E-3 - 4.37E-3 g/cm² | |
Elasticidad de la película | 20.0 °C | 22.89 - 73.26 m²/kg Show Supplier Material materials with Elasticidad de la película of 22.89 - 73.26 m²/kg |
Información de materiales
Property | Value |
---|---|
Medidas | Available thicknesses: 15, 18, 20, 25, 30, 35, 40, 48µm. |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 20.0 °C | 200 - 220 % Show Supplier Material materials with Elongación of 200 - 220 % | GOST 14236, ISO 527, ASTM D882 |
Elongación transversal | 20.0 °C | 70 - 80 % Show Supplier Material materials with Elongación transversal of 70 - 80 % | GOST 14236, ISO 527, ASTM D882 |
Resistencia a la tracción | 20.0 °C | 130 - 140 MPa Show Supplier Material materials with Resistencia a la tracción of 130 - 140 MPa | GOST 14236, ISO 527, ASTM D882 |
Resistencia a la tracción transversal | 20.0 °C | 230 - 250 MPa Show Supplier Material materials with Resistencia a la tracción transversal of 230 - 250 MPa | GOST 14236, ISO 527, ASTM D882 |
Medidas
Property | Value |
---|---|
Espesor | 0.02 - 0.05 mm Show Supplier Material materials with Espesor of 0.02 - 0.05 mm |
Óptico
Property | Value | Comment |
---|---|---|
Turbidez | 2.3 - 3 % Show Supplier Material materials with Turbidez of 2.3 - 3 % | GOST 15875, ISO 14782, ASTM D 1003 |
Technological properties
Property | ||
---|---|---|
Application areas | High quality solvent based rotogravure and flexographic printing; solvent based and solvent free lamination with polyurethane adhesives; manufacture of flexible packaging for food products; for vertical VFFS packaging machines as film in laminate, turned to pulling belts; for horizontal HFFS packaging machines as internal film in laminate (turned to the product); production of decorative packaging for flowers, gift wrap and etc.; for cold seal glue frame coating onto UT film side (if necessary). | |
Friction | Kinetic coefficient of friction µ= 0.2-0.45 (GOST 27492, ISO 8295, ASTM D 1894). | |
Other | HGSL BOPP films comprise: A treated modified heat sealable copolymer skin layer, a transparent oriented polypropylene core layer, a heat sealable, non treated skin layer with low seal intention temperature and standard coefficient of friction. | |
Processing history | Treatment level: 38 mN/m (ISO 8296, ASTM D 2578). |