General
Property | Value | Comment |
---|---|---|
Tamaño de partícula D50 | 0.8 - 1 μm Show Supplier Material materials with Tamaño de partícula D50 of 0.8 - 1 μm | |
Área superficial específica | 12 - 17 m²/g Show Supplier Material materials with Área superficial específica of 12 - 17 m²/g | measured with the BET-method |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminio | 0.01 % Show Supplier Material materials with Aluminio of 0.01 % | Al₂O₃ |
Circonio | 86.2 - 86.6 % Show Supplier Material materials with Circonio of 86.2 - 86.6 % | ZrO₂ |
Cloro | 0.03 - 0.08 % Show Supplier Material materials with Cloro of 0.03 - 0.08 % | |
Hierro | 3E-3 % Show Supplier Material materials with Hierro of 3E-3 % | Fe₂O₃ |
Itrio | 13.3 - 13.7 % Show Supplier Material materials with Itrio of 13.3 - 13.7 % | Y₂O₃ |
Silicona | 0.02 % Show Supplier Material materials with Silicona of 0.02 % | SiO₂ |
Sodio | 0.01 % Show Supplier Material materials with Sodio of 0.01 % | Na₂O |
Titanio | 0.01 % Show Supplier Material materials with Titanio of 0.01 % | TiO₂ |
Technological properties
Property | ||
---|---|---|
Application areas | YSZ powder is suitable for production of different structure ceramics,electronic ceramics,biological ceramics,advanced refractory,optical communication device,man-made jewelry,sensor ,solid fuel battery,grinding and polish trade and so on. Structural Ceramics: since nano ZrO2 ceramics with high toughness, high flexural strength and high wear resistance, excellent thermal insulation properties, thermal expansion coefficient close to steel, etc., nano ZrO2 powder is widely used in the field of structural ceramics. |