General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 4.56 g/cm³ Show Supplier Material materials with Densidad of 4.56 g/cm³ |
Tamaño de partícula D50 | 1.4 - 1.6 μm Show Supplier Material materials with Tamaño de partícula D50 of 1.4 - 1.6 μm |
Chemical properties
Property | Value | Comment |
---|---|---|
Circonio | 64.5 - 65.5 % Show Supplier Material materials with Circonio of 64.5 - 65.5 % | ZrO₂ |
Hierro | 0.1 % Show Supplier Material materials with Hierro of 0.1 % | Fe₂O₃ |
Titanio | 0.15 % Show Supplier Material materials with Titanio of 0.15 % | TiO₂ |
Technological properties
Property | ||
---|---|---|
Application areas | Plastic industry,Refractory materials,as emulsifying agent used in various types of ceramic glaze,coffee cups for export,sanitary ceramics,floor tiles,building tiles.It also can be used in making ceramics rollers and brake discs. Used for epoxy resin formulations,the sealing resin,silicones,vinyl resins,and as the filler material of resin in order to increase the heat resistance and improve the insulation value and it also used in filler materials that requires inert, fine, white and chemical resistant. Casted refractories for glass melting furnaces, heat resistant porcelain, sand flushing in refractory casting and the refractory slabs, special fire resistant porcelain, refractory cement. |