General
Property | Temperature | Value | Comment |
---|---|---|---|
Bio-based content | 40.0 % Show Supplier Material materials with Bio-based content of 40.0 % | ||
Densidad | 23 °C | 1.06 g/cm³ Show Supplier Material materials with Densidad of 1.06 g/cm³ | ISO 1183 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23 °C | 3.5 % Show Supplier Material materials with Elongación of 3.5 % | ISO 527-2/50 |
Módulo de flexión | 23 °C | 4 GPa Show Supplier Material materials with Módulo de flexión of 4 GPa | ISO 527-2/2 |
Módulo elástico | 23 °C | 4.2 GPa Show Supplier Material materials with Módulo elástico of 4.2 GPa | ISO 527-2/2 |
Resistencia a la tracción | 23 °C | 49 MPa Show Supplier Material materials with Resistencia a la tracción of 49 MPa | ISO 527-2/50 |
Resistencia al choque, ensayo Charpy no entallado | 23 °C | 21 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 21 kJ/m² | ISO 179/1eU |
Aplicaciones térmicas
Property | Value |
---|---|
Inflamabilidad | UL94: HB |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Velocidad de flujo de la masa derretida | 23 °C | 15 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 15 g/10min | ISO 1133, 220°C/5kg |
Technological properties
Property | ||
---|---|---|
Certifications | ||
Fillers | 40% S-Wood Fiber | |
Other | General safety instructions, read also Process instructions: | |
Processing methods | Drying: 4 hours at 105°C Injection moulding machine Temperatures: The below instructions may differ on due to injection speed, machine etc. Read process intructions. |