General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 0.38 % Show Supplier Material materials with Absorción de agua of 0.38 % | ASTM D570, 24hr and 50%RH |
Densidad | 23.0 °C | 1.25 g/cm³ Show Supplier Material materials with Densidad of 1.25 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 10 % Show Supplier Material materials with Elongación of 10 % | ASTM D638 |
Impact strength, Izod notched, ASTM | 23.0 °C | 5.1 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 5.1 J/m | ASTM D256 |
Módulo de flexión | 23.0 °C | 4.89 GPa Show Supplier Material materials with Módulo de flexión of 4.89 GPa | ASTM D790 |
Resistencia a la flexión | 23.0 °C | 160 MPa Show Supplier Material materials with Resistencia a la flexión of 160 MPa | ASTM D790 |
Resistencia a la tracción | 23.0 °C | 105 MPa Show Supplier Material materials with Resistencia a la tracción of 105 MPa | ASTM D638 |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Heat deflection temperature, 1.80 MPa | 140 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 140 °C | ASTM D648 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Surface resistivity | 23.0 °C | 10000 - 1000000 Ω/sq Show Supplier Material materials with Surface resistivity of 10000 - 1000000 Ω/sq | ASTM D257 |
Rheological Properties
Property | Value | Comment |
---|---|---|
Velocidad de flujo de la masa derretida | 10 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 10 g/10min | ASTM D2240, 180°C/5kg |
Technological properties
Property | ||
---|---|---|
Certifications | RoHS | |
Color | Black | |
Processing methods | Injection molding - Drying time: 4hrs, temperature: 140°C - mold temperature: 130-160°C - injection temperature: 250-290°C |