General
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 8 % Show Supplier Material materials with Elongación of 8 % | ASTM D638 |
Impact strength, Izod notched, ASTM | 23.0 °C | 2.6 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 2.6 J/m | ASTM D256 |
Módulo de flexión | 23.0 °C | 10.63 GPa Show Supplier Material materials with Módulo de flexión of 10.63 GPa | ASTM D790 |
Resistencia a la flexión | 23.0 °C | 144 MPa Show Supplier Material materials with Resistencia a la flexión of 144 MPa | ASTM D790 |
Resistencia a la tracción | 23.0 °C | 108 MPa Show Supplier Material materials with Resistencia a la tracción of 108 MPa | ASTM D638 |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Heat deflection temperature, 1.80 MPa | 160 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 160 °C | ASTM D648 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Surface resistivity | 23.0 °C | 10000 - 1000000 Ω/sq Show Supplier Material materials with Surface resistivity of 10000 - 1000000 Ω/sq | ASTM D257 |
Rheological Properties
Property | Value | Comment |
---|---|---|
Velocidad de flujo de la masa derretida | 3.45 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 3.45 g/10min | ASTM D2240, 180°C/5kg |
Technological properties
Property | ||
---|---|---|
Certifications | RoHS | |
Color | Black | |
Fillers | Carbon Fiber | |
Processing methods | Injection molding - Drying time: 4hrs, temperature: 150°C - mold temperature: 130°C - injection temperature: 280-320°C |