ASTM A1008 HSLA Grade 80 Brass-plated

Nombres alternativos y comerciales
Brass electroplated steel
Want to keep this datasheet? Save it now in your required format

Description

Tata Steel offers a range of cold-rolled steel strip products electroplated with brass. These products have excellent performance features and provide a cost-effective alternative to solid brass.


Our brass-plated steel products are used in numerous applications from sporting ammunition to household goods. Their consistent quality enables trouble-free processing.


Our cold-rolled steel strip is manufactured to consistently tight dimensional tolerances. Stringent process control ensures excellent adhesion of the pure brass layer during electroplating. The finished product has a brass layer that is uniform, clean and free of oxides. Our products are available in a choice of surface finish to suit your applications.


Tata Steel’s brass-plated steel strip products offer significant benefits for your processing operations. They have outstanding formability. Their deep-drawing properties enable reliable production of components in demanding shapes.


For added benefits, we can tailor our products to meet your exact processing and end-product requirements.


Main benefits of our brass-plated steel include:
  • end-products of consistent and reliable quality
  • improved end-product performance
  • trouble-free, repeatable processing
  • minimised waste
  • extended tool life
  • control of substrate and base metal properties

  • Related Standards

    Los datos sobre este material han sido proporcionados por TATA Steel.

    A menos que se indique lo contrario, todas las medidas corresponden a condiciones de temperatura ambiente. A menos que se indique lo contrario, se utilizan las unidades del SI.
    Las normas armonizadas son similares a uno o varios estándares del proveedor. Es posible que algunas normas armonizadas se ajusten al estándar original, mientras que otras pueden quedar fuera de su alcance.

    Ashby charts

    Propiedades

    Chemical properties

    PropertyValueComment

    Azufre

    0.025 %

    Show Supplier Material materials with Azufre of 0.025 %

    max.

    Carbono

    0.15 %

    Show Supplier Material materials with Carbono of 0.15 %

    max.

    Cobre

    0.2 %

    Show Supplier Material materials with Cobre of 0.2 %

    max.

    Cromo

    0.15 %

    Show Supplier Material materials with Cromo of 0.15 %

    max.

    Fósforo

    0.02 %

    Show Supplier Material materials with Fósforo of 0.02 %

    max.

    Manganeso

    1.65 %

    Show Supplier Material materials with Manganeso of 1.65 %

    max.

    Molibdeno

    0.16 %

    Show Supplier Material materials with Molibdeno of 0.16 %

    max.

    Níquel

    0.2 %

    Show Supplier Material materials with Níquel of 0.2 %

    max.

    Otro

    0.005 %

    Show Supplier Material materials with Otro of 0.005 %

    min. Cb/Nb

    Titanio

    0.005 %

    Show Supplier Material materials with Titanio of 0.005 %

    min.

    Vanadio

    0.005 %

    Show Supplier Material materials with Vanadio of 0.005 %

    min.

    Technological properties

    Property
    Application areas

  • Sporting ammunition
  • Decorative household products
  • Automotive components

  • Other

    Surface roughness (Ra)
    KR 0 / Appliance FinishRa: ≤ 0.10 μm (exceptionally smooth mirror finish)
    KR 0.5Ra: ≤ 0.20 μm (very smooth bright finish)
    KR 4 / #2 FinishRa: 0.15 - 0.45 μm (smooth finish)
    KR 7 / #1 FinishRa: 0.6 - 1.8 μm (rough finish)
    KR 8 / #1 FinishRa: 1.0 - 2.5 μm (rough matt finish)


    Coil weight
    Strip thickness (mm / inch)max coil weight EU/US
    0.1 – 1.4 / 0.008” – 0.055”10kg/mm coil width (10 KIM) / 700 PIW


    Coil inner diameter (ID)
    mm / inch
    Coil outer diameter (OD)
    mm / inch
    400, 500 / 16”, 20”max. 1368 / 60”


    Coil edge finishes
    Natural edges (#2)strip edges have a mill edge (un-slit edges)
    Slit edges (#3)strip edges have been slit (reduces maximum width by a total of 10mm)
    Sheets cut to lengthstrip cut to a specific length (sheets)
    Straight wound coilsstandard
    Traverse wound coils (a spool)upon request – please consult us


    Delivery conditionThickness range (mm/inch)Plating thickness (μm/µ")Width range (mm/inch)
    LC, C290, C340, C390, C440, C490, C590, C690, 1T (full hard), 2T, 3T, 4T, 5T0.20 – 1.70 / 0.008 - 0.0701.5 - 5.0 / 60 - 2003 - 724 / 0.10 - 28.5

    Packaging size

    Skid Type (2 & 3 runners) Dimensions mm / inch
    Pallet (Eye to sky) Coil Pallet (Eye to the side) 2 - wayMinimum 660 x 660 / 26” x 26”
    4 - wayMaximum 1321 x 1321 / 52” x 52”
    Parameters selected to protect coils from overhanging skids
    Coil No Pallet (Eye to side)Shrouded / Stretch-wrapped


    Other packaging options are available – please consult us.

    Surface Finish

  • Natural brass finish
  • Roughness from smooth to heavy matt
  • Brushed finish

  • Surface protection

  • Our products can be delivered with adhesive protective foils on the surface including among others: oil-resistant PVC foil, PE foil or a special PE foil used for laser-cutting purposes.
  • In addition we apply oil according to your requirements.
  • Other surface protection options are available – please consult us.