Chemical properties
Property | Value | Comment |
---|---|---|
Azufre | 0.025 % Show Supplier Material materials with Azufre of 0.025 % | max. |
Carbono | 0.15 % Show Supplier Material materials with Carbono of 0.15 % | max. |
Cobre | 0.2 % Show Supplier Material materials with Cobre of 0.2 % | max. |
Cromo | 0.15 % Show Supplier Material materials with Cromo of 0.15 % | max. |
Fósforo | 0.02 % Show Supplier Material materials with Fósforo of 0.02 % | max. |
Manganeso | 1.65 % Show Supplier Material materials with Manganeso of 1.65 % | max. |
Molibdeno | 0.16 % Show Supplier Material materials with Molibdeno of 0.16 % | max. |
Níquel | 0.2 % Show Supplier Material materials with Níquel of 0.2 % | max. |
Otro | 0.005 % Show Supplier Material materials with Otro of 0.005 % | min. Cb/Nb |
Titanio | 0.005 % Show Supplier Material materials with Titanio of 0.005 % | min. |
Vanadio | 0.005 % Show Supplier Material materials with Vanadio of 0.005 % | min. |
Technological properties
Property | ||
---|---|---|
Application areas | Battery components: cans, covers, connector strips | |
Other | ||
Packaging size | ||
Surface Finish | ||