General
Property | Value | Comment |
---|---|---|
Densidad | 1.29 g/cm³ Show Supplier Material materials with Densidad of 1.29 g/cm³ | ASTM D792 |
Medidas
Property | Value | Comment |
---|---|---|
Diámetro | 1.75 mm Show Supplier Material materials with Diámetro of 1.75 mm | Tolerance +/- 0.02 mm |
Mecánica
Property | Value | Comment |
---|---|---|
Dureza Shore A | 76.0 [-] Show Supplier Material materials with Dureza Shore A of 76.0 [-] | ASTM D2240 |
Elongación | 29 % Show Supplier Material materials with Elongación of 29 % | ISO 527-2 |
Límite elástico | 51.0 MPa Show Supplier Material materials with Límite elástico of 51.0 MPa | ISO 527-2 |
Módulo de flexión | 2.04 GPa Show Supplier Material materials with Módulo de flexión of 2.04 GPa | ISO 172 |
Módulo elástico | 2.98 GPa Show Supplier Material materials with Módulo elástico of 2.98 GPa | ISO 527-2 |
Resistencia a la flexión | 68 MPa Show Supplier Material materials with Resistencia a la flexión of 68 MPa | ISO 172 |
Resistencia a la tracción | 20 MPa Show Supplier Material materials with Resistencia a la tracción of 20 MPa | ISO 527-2 |
Aplicaciones térmicas
Property | Value | Pressure | Comment |
---|---|---|---|
Temperatura de flexión bajo carga | 68 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 68 °C | 0.45 MPa | ISO 75-2 |
Temperatura de reblandecimiento Vicat | 78.0 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 78.0 °C | ISO 3076 | |
Temperatura de transición del vidrio | 80.0 °C Show Supplier Material materials with Temperatura de transición del vidrio of 80.0 °C | ASTM D3418 |
Technological properties
Property | ||
---|---|---|
Application areas | END-USE PARTS: containers, holders - PROTOTYPES: bottles, packaging - ELECTRONICS: covers, cases, products containing diodes - DECORATIONS: lamps, glass-resembling elements - JEWELLERY: rings, necklaces, bracelets | |
Certifications | Food Contact approved | |
Processing methods | Print temperature: 230-250°C, Bed temperature: 90°C |