General
Property | Value | Comment |
---|---|---|
Densidad | 1.03 g/cm³ Show Supplier Material materials with Densidad of 1.03 g/cm³ | ASTM D792 |
Medidas
Mecánica
Property | Value | Comment |
---|---|---|
Elongación | 30 % Show Supplier Material materials with Elongación of 30 % | ASTM D638 |
Límite elástico | 37.75 MPa Show Supplier Material materials with Límite elástico of 37.75 MPa | ASTM D638 |
Módulo de flexión | 2.15 GPa Show Supplier Material materials with Módulo de flexión of 2.15 GPa | ASTM D790 |
Resistencia a la flexión | 60.81 MPa Show Supplier Material materials with Resistencia a la flexión of 60.81 MPa | ASTM D790 |
Aplicaciones térmicas
Property | Value | Pressure | Comment |
---|---|---|---|
Temperatura de flexión bajo carga | 90 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 90 °C | 1.8 MPa | ASTM D648, unannealed-annealed condition |
95 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 95 °C | 1.8 MPa | ASTM D648, unannealed-annealed condition | |
Temperatura de reblandecimiento Vicat | 103.0 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 103.0 °C | ASTM D1525 |
Rheological Properties
Property | Value | Comment |
---|---|---|
Velocidad de flujo de la masa derretida | 1.1 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 1.1 g/10min | ASTM D1238 , 200°C/5Kg |
Technological properties
Property | ||
---|---|---|
Application areas | PROTOTYPES: linking elements, elements which require high temperature resistance - TOOLS OR THEIR ELEMENTS: gears, racks, elements which require high durability - GADGETS OR THEIR PARTS: phone cases, stands, keychains - TOYS: bricks, robots or their parts, car elements - HOUSE EQUIPMENT: hangers, flower pots, vases | |
Processing methods | Bed heating required, chamber heating is not required but when using we suggest to keep 80°C. Printing temperature: 250-265°C, Bed temperature: 90-110°C |