General
Property | Value | Comment |
---|---|---|
Absorción de agua | 0.8 % Show Supplier Material materials with Absorción de agua of 0.8 % | ASTM D570 |
Densidad | 1.07 g/cm³ Show Supplier Material materials with Densidad of 1.07 g/cm³ |
Medidas
Property | Value | Comment |
---|---|---|
Diámetro | 1.75 mm Show Supplier Material materials with Diámetro of 1.75 mm | Tolerance +/- 0.05 mm |
Mecánica
Property | Value | Comment |
---|---|---|
Dureza Shore D | 30.0 [-] Show Supplier Material materials with Dureza Shore D of 30.0 [-] | ASTM D2240 |
Elongación | 900 % Show Supplier Material materials with Elongación of 900 % | ASTM D638 |
Módulo de flexión | 0.066 GPa Show Supplier Material materials with Módulo de flexión of 0.066 GPa | ASTM D790 |
Rebound Resilience | 72.0 % Show Supplier Material materials with Rebound Resilience of 72.0 % | ASTM D2632 |
Resistencia a desgarros | 95.0 kN/m Show Supplier Material materials with Resistencia a desgarros of 95.0 kN/m | ASTM D1004 |
Resistencia a la tracción | 21.57 MPa Show Supplier Material materials with Resistencia a la tracción of 21.57 MPa | ASTM D638 |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Temperatura de fusión | 174.0 °C Show Supplier Material materials with Temperatura de fusión of 174.0 °C | ASTM D3418 |
Technological properties
Property | ||
---|---|---|
Application areas | RUBBER ELEMENTS OF MACHINES: Polymer Gaskets, elements that are frequently bent - GADGETS OR THEIR ELEMENTS: phone sleeves and cases, watch-, pulse counter-, pedometer straps - LINKING ELEMENTS: flexible hinges - TOYS OR THEIR ELEMENTS: tires, rubber figures - JEWELLERY: bands, bracelets | |
Processing methods | Print temperature: 200 – 220°C, bed temperature: 50 – 70 °C - to remove the print easier, it is recommended to heat the bed to 110°C |