General
Property | Value | Comment |
---|---|---|
Densidad | 1.24 - 1.25 g/cm³ Show Supplier Material materials with Densidad of 1.24 - 1.25 g/cm³ | ISO 1183 (Maximum value is reached through annealing) |
Medidas
Mecánica
Property | Value | Comment |
---|---|---|
Elongación | 2.4 - 2.7 % Show Supplier Material materials with Elongación of 2.4 - 2.7 % | ISO 178(Minimum value is reached through annealing) |
Módulo de flexión | 3.43 GPa Show Supplier Material materials with Módulo de flexión of 3.43 GPa | ISO 178(Maximum value is reached through annealing) |
3.435 GPa Show Supplier Material materials with Módulo de flexión of 3.435 GPa | ISO 178(Maximum value is reached through annealing) | |
Módulo elástico | 3.65 - 3.71 GPa Show Supplier Material materials with Módulo elástico of 3.65 - 3.71 GPa | ISO 527 (Maximum value is reached through annealing) |
Resistencia a la flexión | 90.0 - 93.0 MPa Show Supplier Material materials with Resistencia a la flexión of 90.0 - 93.0 MPa | ISO 178(Maximum value is reached through annealing) |
Resistencia a la tracción | 45.0 - 51.0 MPa Show Supplier Material materials with Resistencia a la tracción of 45.0 - 51.0 MPa | ISO 527 (Maximum value is reached through annealing) |
Resistencia al choque, ensayo Charpy no entallado | 11 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 11 kJ/m² | ISO 179-1 (Maximum value is reached through annealing) |
20 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 20 kJ/m² | ISO 179-1 (Maximum value is reached through annealing) |
Aplicaciones térmicas
Property | Value | Pressure | Comment |
---|---|---|---|
Temperatura de flexión bajo carga | 80 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 80 °C | 1.8 MPa | ISO 75, unannealed-annealed condition |
144 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 144 °C | 1.8 MPa | ISO 75, unannealed-annealed condition |
Technological properties
Property | ||
---|---|---|
Application areas | TOYS OR THEIR ELEMENTS: human figures, animals, constructions, houses, vehicles, dice - GADGETS OR THEIR ELEMENTS: key rings, stands, phone cases - PROTOTYPES: tools, concept models - ELEMENTS OF JEWELLERY: earrings, bracelets, beads, necklaces - SPARE PARTS: elements of machines, equipment, vehicles, electronic equipment - TOOLS: complex elements requiring durability - HOUSE EQUIPMENT: bowls, trays, boxes | |
Processing methods | Print temperature: 200-230°C, Bed temperature: 50-70°C (when using plates or other means to increase the adhesion, the heating of the bed is not required) - heating of the print should be conducted in accordance with the manual provided by Fiberlogy |