General
Property | Value |
---|---|
Densidad | 1.4 g/cm³ Show Supplier Material materials with Densidad of 1.4 g/cm³ |
Medidas
Mecánica
Aplicaciones térmicas
Property | Value | Pressure |
---|---|---|
Temperatura de flexión bajo carga | 48 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 48 °C | 0.45 MPa |
Rheological Properties
Property | Value | Comment |
---|---|---|
Velocidad de flujo del volumen derretido | 16.0 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 16.0 cm³/10min | 190°C/2.16Kg |
Technological properties
Property | ||
---|---|---|
Application areas | MODELS: buildings, structures, land development projects, interiors - DECORATIONS: statues, sculptures, reliefs - MODELING: small elements requiring high precision - PROTOTYPES: concept models, small parts | |
Processing methods | Print temperature: 190-210°C, Bed temperature: 50-70°C (when using plates or other means to increase the adhesion, the heating of the bed is not required) |