General
Property | Value |
---|---|
Densidad aparente | 4.65 - 4.8 g/cm³ Show Supplier Material materials with Densidad aparente of 4.65 - 4.8 g/cm³ |
Tamaño de partícula D10 | 20.0 - 25.0 μm Show Supplier Material materials with Tamaño de partícula D10 of 20.0 - 25.0 μm |
Tamaño de partícula D50 | 33.0 - 35.0 μm Show Supplier Material materials with Tamaño de partícula D50 of 33.0 - 35.0 μm |
Tamaño de partícula D90 | 43.0 - 45.0 μm Show Supplier Material materials with Tamaño de partícula D90 of 43.0 - 45.0 μm |
Rheological Properties
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminio | 0.61 % Show Supplier Material materials with Aluminio of 0.61 % | |
Azufre | 0.001 % Show Supplier Material materials with Azufre of 0.001 % | Maximum |
Boro | 0.005 % Show Supplier Material materials with Boro of 0.005 % | Maximum |
Carbono | 0.02 % Show Supplier Material materials with Carbono of 0.02 % | |
Cobalto | 0.17 % Show Supplier Material materials with Cobalto of 0.17 % | |
Cobre | 0.04 % Show Supplier Material materials with Cobre of 0.04 % | |
Cromo | 17.6 % Show Supplier Material materials with Cromo of 17.6 % | |
Fósforo | 0.005 % Show Supplier Material materials with Fósforo of 0.005 % | |
Hidrógeno | 0.0004 % Show Supplier Material materials with Hidrógeno of 0.0004 % | |
Hierro | 18.5 % Show Supplier Material materials with Hierro of 18.5 % | |
Manganeso | 0.07 % Show Supplier Material materials with Manganeso of 0.07 % | |
Molibdeno | 2.89 % Show Supplier Material materials with Molibdeno of 2.89 % | |
Niobio | 5.14 % Show Supplier Material materials with Niobio of 5.14 % | |
Nitrógeno | 0.01 % Show Supplier Material materials with Nitrógeno of 0.01 % | |
Níquel | 54.17 % Show Supplier Material materials with Níquel of 54.17 % | |
Oxígeno | 0.01 % Show Supplier Material materials with Oxígeno of 0.01 % | |
Silicona | 0.07 % Show Supplier Material materials with Silicona of 0.07 % | |
Titanio | 0.97 % Show Supplier Material materials with Titanio of 0.97 % | |
Vanadio | 0.04 % Show Supplier Material materials with Vanadio of 0.04 % | |
Wolframio | 0.03 % Show Supplier Material materials with Wolframio of 0.03 % |
Technological properties
Property | ||
---|---|---|
Application areas | Additive manufacturing, Metal Injection Molding, Thermal Spray, Biomedical, Aerospace |