General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 7.98 g/cm³ Show Supplier Material materials with Densidad of 7.98 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Elongación | 23.0 °C | 40 % Show Supplier Material materials with Elongación of 40 % |
Límite elástico | 23.0 °C | 205 MPa Show Supplier Material materials with Límite elástico of 205 MPa |
Resistencia a la tracción | 23.0 °C | 515 MPa Show Supplier Material materials with Resistencia a la tracción of 515 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.03 % Show Supplier Material materials with Azufre of 0.03 % |
Carbono | 0.08 % Show Supplier Material materials with Carbono of 0.08 % |
Cromo | 24 - 26 % Show Supplier Material materials with Cromo of 24 - 26 % |
Fósforo | 0.05 % Show Supplier Material materials with Fósforo of 0.05 % |
Manganeso | 2 % Show Supplier Material materials with Manganeso of 2 % |
Níquel | 19 - 22 % Show Supplier Material materials with Níquel of 19 - 22 % |
Silicona | 1.5 % Show Supplier Material materials with Silicona of 1.5 % |
Technological properties
Property | ||
---|---|---|
Application areas | Pressure Vessel& Anti-Corrosion Building |