General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 7.93 g/cm³ Show Supplier Material materials with Densidad of 7.93 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Elongación | 23.0 °C | 40 % Show Supplier Material materials with Elongación of 40 % |
Límite elástico | 23.0 °C | 205 MPa Show Supplier Material materials with Límite elástico of 205 MPa |
Resistencia a la tracción | 23.0 °C | 515 MPa Show Supplier Material materials with Resistencia a la tracción of 515 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.03 % Show Supplier Material materials with Azufre of 0.03 % |
Carbono | 0.04 - 0.1 % Show Supplier Material materials with Carbono of 0.04 - 0.1 % |
Cromo | 18 - 20 % Show Supplier Material materials with Cromo of 18 - 20 % |
Fósforo | 0.05 % Show Supplier Material materials with Fósforo of 0.05 % |
Manganeso | 2 % Show Supplier Material materials with Manganeso of 2 % |
Níquel | 8 - 10.5 % Show Supplier Material materials with Níquel of 8 - 10.5 % |
Silicona | 0.75 % Show Supplier Material materials with Silicona of 0.75 % |
Technological properties
Property | ||
---|---|---|
Application areas | Pressure Vessel& Anti-Corrosion Building |