General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 0.1 % Show Supplier Material materials with Absorción de agua of 0.1 % | maximum, ASTM D570 |
Densidad | 23.0 °C | 1.04 g/cm³ Show Supplier Material materials with Densidad of 1.04 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 35 % Show Supplier Material materials with Elongación of 35 % | ASTM D638 |
Hardness, Rockwell L | 23.0 °C | 50 [-] Show Supplier Material materials with Hardness, Rockwell L of 50 [-] | ASTM D785 |
Módulo de flexión | 23.0 °C | 1.91 GPa Show Supplier Material materials with Módulo de flexión of 1.91 GPa | ASTM D790 |
Resistencia a la flexión | 23.0 °C | 45.1 MPa Show Supplier Material materials with Resistencia a la flexión of 45.1 MPa | ASTM D 790 |
Resistencia a la tracción | 23.0 °C | 24.52 MPa Show Supplier Material materials with Resistencia a la tracción of 24.52 MPa | ASTM D638 |
Aplicaciones térmicas
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 83 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 83 °C | ASTM D648 | |
Temperatura de reblandecimiento Vicat | 106 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 106 °C | ASTM D1525 | |
Inflamabilidad | HB UL94 |
Rheological Properties
Property | Value | Comment |
---|---|---|
Velocidad de flujo de la masa derretida | 8.5 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 8.5 g/10min | ASTM D1238 |
Technological properties
Property | ||
---|---|---|
Application areas | Compounding grades |