General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.04 g/cm³ Show Supplier Material materials with Densidad of 1.04 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 40 % Show Supplier Material materials with Elongación of 40 % | ASTM D638 |
Hardness, Rockwell R | 23.0 °C | 108 [-] Show Supplier Material materials with Hardness, Rockwell R of 108 [-] | ASTM D785 |
Límite elástico | 23.0 °C | 45.1 MPa Show Supplier Material materials with Límite elástico of 45.1 MPa | ASTM D638 |
Módulo de flexión | 23.0 °C | 2.45 GPa Show Supplier Material materials with Módulo de flexión of 2.45 GPa | ASTM D790 |
Módulo elástico | 23.0 °C | 2.08 GPa Show Supplier Material materials with Módulo elástico of 2.08 GPa | ASTM D638 |
Resistencia a la flexión | 23.0 °C | 72.6 MPa Show Supplier Material materials with Resistencia a la flexión of 72.6 MPa | ASTM D790 |
Aplicaciones térmicas
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 0.45 MPa | 91 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 91 °C | ASTM D648 | |
Heat deflection temperature, 1.80 MPa | 87 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 87 °C | ASTM D648 | |
Relative temperature index, electrical | 60 °C Show Supplier Material materials with Relative temperature index, electrical of 60 °C | UL 746B | |
Relative temperature index, mechanical impact | 60 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 60 °C | UL 746B | |
Relative temperature index, mechanical strength | 60 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 60 °C | UL 746B | |
Temperatura de reblandecimiento Vicat | 93 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 93 °C | ASTM D1525 | |
Inflamabilidad | HB UL94 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Índice de seguimiento comparativo | 23.0 °C | 0 V Show Supplier Material materials with Índice de seguimiento comparativo of 0 V | IEC 60112 |
Rheological Properties
Property | Value | Comment |
---|---|---|
Velocidad de flujo de la masa derretida | 21 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 21 g/10min | ASTM D1238 |
Technological properties
Property | ||
---|---|---|
Application areas | ELECTRIC & ELECTRONIC, MISCELLANEOUS GOODS |