General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 0.1 % Show Supplier Material materials with Absorción de agua of 0.1 % | maximum, ASTM D570 |
Densidad | 23.0 °C | 1.04 g/cm³ Show Supplier Material materials with Densidad of 1.04 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 2 % Show Supplier Material materials with Elongación of 2 % | ASTM D638 |
Hardness, Rockwell L | 23.0 °C | 70 [-] Show Supplier Material materials with Hardness, Rockwell L of 70 [-] | ASTM D785 |
Límite elástico | 23.0 °C | 45 MPa Show Supplier Material materials with Límite elástico of 45 MPa | ASTM D638 |
Módulo de flexión | 23.0 °C | 3.24 GPa Show Supplier Material materials with Módulo de flexión of 3.24 GPa | ASTM D790 |
Resistencia al choque, ensayo Izod no entallado | 23.0 °C | 7.5 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod no entallado of 7.5 kJ/m² | ISO 180 |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 7.1E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 7.1E-5 1/K | ASTM D696 |
Heat deflection temperature, 1.80 MPa | 75 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 75 °C | ASTM D648 | |
Temperatura de reblandecimiento Vicat | 91 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 91 °C | ASTM D1525 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Rigidez dieléctrica | 23.0 °C | 135 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 135 kV/mm | ASTM D149 |
Surface resistivity | 23.0 °C | 1.00E+13 Ω/sq Show Supplier Material materials with Surface resistivity of 1.00E+13 Ω/sq | IEC 93 |
Rheological Properties
Property | Value | Comment |
---|---|---|
Velocidad de flujo de la masa derretida | 12 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 12 g/10min | ASTM D1238 |
Technological properties
Property | ||
---|---|---|
Application areas | CUTLERY, JEWEL BOX, TOY |