General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 0.07 % Show Supplier Material materials with Absorción de agua of 0.07 % | ASTM D570 |
Densidad | 23.0 °C | 1.04 g/cm³ Show Supplier Material materials with Densidad of 1.04 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 40 % Show Supplier Material materials with Elongación of 40 % | ASTM D638 |
Hardness, Rockwell R | 23.0 °C | 99 [-] Show Supplier Material materials with Hardness, Rockwell R of 99 [-] | ASTM D785 |
Límite elástico | 23.0 °C | 31 MPa Show Supplier Material materials with Límite elástico of 31 MPa | ASTM D638 |
Módulo de flexión | 23.0 °C | 2.3 GPa Show Supplier Material materials with Módulo de flexión of 2.3 GPa | ASTM D790 |
Resistencia al choque, ensayo Izod no entallado | 23.0 °C | 9.5 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod no entallado of 9.5 kJ/m² | ISO 180 |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 9.05E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 9.05E-5 1/K | ASTM D696 |
Heat deflection temperature, 1.80 MPa | 80 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 80 °C | ASTM D648 | |
Temperatura de reblandecimiento Vicat | 98 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 98 °C | ASTM D1525 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Rigidez dieléctrica | 23.0 °C | 150 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 150 kV/mm | ASTM D149 |
Surface resistivity | 23.0 °C | 1.00E+13 Ω/sq Show Supplier Material materials with Surface resistivity of 1.00E+13 Ω/sq | IEC 93 |
Rheological Properties
Property | Value | Comment |
---|---|---|
Velocidad de flujo de la masa derretida | 8 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 8 g/10min | ASTM D1238 |
Technological properties
Property | ||
---|---|---|
Application areas | TV COVER, OFFICE AUTOMATION, ELECTRIC & ELECTRONIC, HOUSEHOLD |