General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 0.1 % Show Supplier Material materials with Absorción de agua of 0.1 % | maximum, ASTM D570 |
Densidad | 23.0 °C | 1.04 g/cm³ Show Supplier Material materials with Densidad of 1.04 g/cm³ | ISO 1183 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Hardness, Rockwell L | 23.0 °C | 56 [-] Show Supplier Material materials with Hardness, Rockwell L of 56 [-] | ASTM D785 |
Módulo de flexión | 23.0 °C | 2.03 GPa Show Supplier Material materials with Módulo de flexión of 2.03 GPa | ISO 178 |
Resistencia a la flexión | 23.0 °C | 50 MPa Show Supplier Material materials with Resistencia a la flexión of 50 MPa | ISO 178 |
Resistencia a la tracción | 23.0 °C | 28 MPa Show Supplier Material materials with Resistencia a la tracción of 28 MPa | ISO 527-1 |
Resistencia al choque, ensayo Charpy entallado | 23.0 °C | 13 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 13 kJ/m² | ISO 179 |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 5E-5 - 1E-4 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 5E-5 - 1E-4 1/K | ASTM D696 | ||
Heat deflection temperature, 0.45 MPa | 78 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 78 °C | ISO 75 | |||
Relative temperature index, electrical | 50 °C Show Supplier Material materials with Relative temperature index, electrical of 50 °C | UL 746B | |||
Relative temperature index, mechanical impact | 50 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 50 °C | UL 746B | |||
Relative temperature index, mechanical strength | 50 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 50 °C | UL 746B | |||
Inflamabilidad | HB UL94 |
Rheological Properties
Property | Value | Comment |
---|---|---|
Velocidad de flujo de la masa derretida | 2.5 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 2.5 g/10min | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Application areas | SHEET EXTRUSION & THERMOFORMING, TAPE REEL & BOBBIN, DISPOSABLE CUPS & PLATES & TRAYS |