General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.2 g/cm³ Show Supplier Material materials with Densidad of 1.2 g/cm³ | ISO 1183 |
Mecánica
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Elongación | 23.0 °C | 50 % Show Supplier Material materials with Elongación of 50 % | ISO 527-2/50 | ||
Elongation at yield | 23.0 °C | 6 % Show Supplier Material materials with Elongation at yield of 6 % | ISO 527-2/50 | ||
Límite elástico | 23.0 °C | 61 MPa Show Supplier Material materials with Límite elástico of 61 MPa | ISO 527-2/50 | ||
Módulo de flexión | 23.0 °C | 2.35 GPa Show Supplier Material materials with Módulo de flexión of 2.35 GPa | ISO 178 | ||
Módulo elástico | 23.0 °C | 2.4 GPa Show Supplier Material materials with Módulo elástico of 2.4 GPa | ISO 527-2/1 | ||
Resistencia a la flexión | 23.0 °C | 93 MPa Show Supplier Material materials with Resistencia a la flexión of 93 MPa | ISO 178 | ||
Resistencia al choque, ensayo Charpy entallado | 23.0 °C | 67 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 67 kJ/m² | ISO 179 | ||
Resistencia al choque, ensayo Charpy no entallado | ISO 179, no break |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 7.5E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 7.5E-5 1/K | ISO 11359-2 | ||
Heat deflection temperature, 0.45 MPa | 139 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 139 °C | ISO 75-2/B | |||
Heat deflection temperature, 1.80 MPa | 126 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 126 °C | ISO 75-2/A | |||
Relative temperature index, electrical | 125 °C Show Supplier Material materials with Relative temperature index, electrical of 125 °C | UL 746 | |||
Relative temperature index, mechanical impact | 115 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 115 °C | UL 746 | |||
Relative temperature index, mechanical strength | 125 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 125 °C | UL 746 | |||
Temperatura de reblandecimiento Vicat | 146 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 146 °C | ISO 306/B50 | |||
Inflamabilidad | HB for 1.9mm and V-2 for 0.4mm UL94 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Constante dieléctrica, 1 MHz | 23.0 °C | 3 [-] Show Supplier Material materials with Constante dieléctrica, 1 MHz of 3 [-] | IEC 60250 |
Constante dieléctrica, 100 Hz | 23.0 °C | 3.1 [-] Show Supplier Material materials with Constante dieléctrica, 100 Hz of 3.1 [-] | IEC 60250 |
Dissipation factor, 100Hz | 23.0 °C | 1E-3 [-] Show Supplier Material materials with Dissipation factor, 100Hz of 1E-3 [-] | IEC 60250 |
Dissipation factor, 1MHz | 23.0 °C | 9E-3 [-] Show Supplier Material materials with Dissipation factor, 1MHz of 9E-3 [-] | IEC 60250 |
Resistividad eléctrica | 23.0 °C | 1.00E+13 Ω·m Show Supplier Material materials with Resistividad eléctrica of 1.00E+13 Ω·m | IEC 60093 |
Rigidez dieléctrica | 23.0 °C | 30 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 30 kV/mm | IEC 60243-1 |
Surface resistivity | 23.0 °C | 1.00E+15 Ω/sq Show Supplier Material materials with Surface resistivity of 1.00E+15 Ω/sq | IEC 60093 |
Índice de seguimiento comparativo | 23.0 °C | 250 V Show Supplier Material materials with Índice de seguimiento comparativo of 250 V | IEC 60112 |
Óptico
Rheological Properties
Property | Value | Comment |
---|---|---|
Velocidad de flujo de la masa derretida | 18 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 18 g/10min | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Application areas | GENERAL PURPOSE |