General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.27 g/cm³ Show Supplier Material materials with Densidad of 1.27 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 180 % Show Supplier Material materials with Elongación of 180 % | ASTM D638 |
Elongation at yield | 23.0 °C | 4.5 % Show Supplier Material materials with Elongation at yield of 4.5 % | ASTM D638 |
Hardness, Rockwell R | 23.0 °C | 108 [-] Show Supplier Material materials with Hardness, Rockwell R of 108 [-] | ASTM D785 |
Límite elástico | 23.0 °C | 50 MPa Show Supplier Material materials with Límite elástico of 50 MPa | ASTM D638 |
Módulo de flexión | 23.0 °C | 2.1 GPa Show Supplier Material materials with Módulo de flexión of 2.1 GPa | ASTM D790 |
Resistencia a la flexión | 23.0 °C | 69 MPa Show Supplier Material materials with Resistencia a la flexión of 69 MPa | ASTM D790 |
Resistencia a la tracción | 23.0 °C | 29 MPa Show Supplier Material materials with Resistencia a la tracción of 29 MPa | ASTM D638 |
Resistencia al choque, ensayo Charpy entallado | 23.0 °C | 105 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 105 kJ/m² | ASTM D 256 |
Aplicaciones térmicas
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 0.45 MPa | 70 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 70 °C | ASTM D648 | |
Heat deflection temperature, 1.80 MPa | 62 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 62 °C | ASTM D648 | |
Inflamabilidad | HB for 1.9mm and V-2 for 0.4mm UL94 |
Óptico
Property | Value | Comment |
---|---|---|
Transmission | 90 % Show Supplier Material materials with Transmission of 90 % | ASTM D1003 at 3000 μm |
Technological properties
Property | ||
---|---|---|
Application areas | Sheet, Cosmetic, Construction, Food, Drink, Deco Film |