General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 4.3 - 4.9 g/cm³ Show Supplier Material materials with Densidad of 4.3 - 4.9 g/cm³ | |
Tamaño de partícula D50 | 7 - 30 μm Show Supplier Material materials with Tamaño de partícula D50 of 7 - 30 μm | ||
Tamaño de partícula D90 | 15 - 40 μm Show Supplier Material materials with Tamaño de partícula D90 of 15 - 40 μm | ||
Volatile share | 0.5 % Show Supplier Material materials with Volatile share of 0.5 % | at 105°C |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 324 J/(kg·K) Show Supplier Material materials with Calor específico of 324 J/(kg·K) | |
Conductividad térmica | 23.0 °C | 1.13 W/(m·K) Show Supplier Material materials with Conductividad térmica of 1.13 W/(m·K) | |
Difusividad térmica | 23.0 °C | 1.34 mm²/s Show Supplier Material materials with Difusividad térmica of 1.34 mm²/s | |
Límite de oxidación | 400 °C Show Supplier Material materials with Límite de oxidación of 400 °C | min. | |
Temperatura de fusión | 1100 °C Show Supplier Material materials with Temperatura de fusión of 1100 °C | ||
Temperatura máx. de funcionamiento | 400 °C Show Supplier Material materials with Temperatura máx. de funcionamiento of 400 °C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 23.0 °C | 140000 S/m Show Supplier Material materials with Conductividad eléctrica of 140000 S/m |
Resistividad eléctrica | 23.0 °C | 7E-6 Ω·m Show Supplier Material materials with Resistividad eléctrica of 7E-6 Ω·m |
Technological properties
Property | ||
---|---|---|
Application areas | Tribotecc® CB 500 Copper-(II)-sulfide is characterised by its excellent absorbens and catalytical properties. Combined with the ability to form stable layers of different contact surfaces over a wide range of temperatures and pressures and excellent wear and friction properties as an additive, this product is ideal for a wide range of applications: E.g. in the areas of: | |
Color | Blue, Black |