Description

GREENETHENE G-3645UV is a Low Density Linear Polyethylene Resin (LLDPE) in powder form, additivated with antioxidants and UV stabilizers. It is suitable for Rotational Molding applications. Items produced by GREENETHENE G-3645UV have a very good balance between mechanical properties and ESCR resistance. G-3645UV is produced in: natural, black, terracotta, fire red, yellow & blue. GREENETHENE G-3645UV meets the requirement stipulated in standard IS:10141:2001 on “Specification for Polyethylene for safe use in contact with foodstuff, pharmaceuticals & Drinking Water”. It also conforms to IS 12701:1996 –“Specification For Rotational Moulded Polyethylene Water Storage Tanks.”.

Los datos sobre este material han sido proporcionados por GreenAge Industries.

A menos que se indique lo contrario, todas las medidas corresponden a condiciones de temperatura ambiente. A menos que se indique lo contrario, se utilizan las unidades del SI.
Las normas armonizadas son similares a uno o varios estándares del proveedor. Es posible que algunas normas armonizadas se ajusten al estándar original, mientras que otras pueden quedar fuera de su alcance.

Ashby charts

Propiedades

General

PropertyTemperatureValueComment

Densidad

23.0 °C

0.94 g/cm³

Show Supplier Material materials with Densidad of 0.94 g/cm³

ASTM D1505

Mecánica

PropertyTemperatureValueComment

Dureza Shore D

23.0 °C

55 [-]

Show Supplier Material materials with Dureza Shore D of 55 [-]

ASTM D2240

Elongación

23.0 °C

165 - 600 %

Show Supplier Material materials with Elongación of 165 - 600 %

ASTM D638

Impact strength, Izod notched, ASTM

23.0 °C

250 J/m

Show Supplier Material materials with Impact strength, Izod notched, ASTM of 250 J/m

ASTM D256

Límite elástico

23.0 °C

17.5 - 18 MPa

Show Supplier Material materials with Límite elástico of 17.5 - 18 MPa

ASTM D638

Módulo de flexión

23.0 °C

0.23 - 0.59 GPa

Show Supplier Material materials with Módulo de flexión of 0.23 - 0.59 GPa

ASTM D790

Resistencia a la tracción

23.0 °C

11.75 MPa

Show Supplier Material materials with Resistencia a la tracción of 11.75 MPa

ASTM D638

Aplicaciones térmicas

PropertyValueComment

Temperatura de reblandecimiento Vicat

117 °C

Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 117 °C

ASTM D1525

Rheological Properties

PropertyValueComment

Velocidad de flujo de la masa derretida

4.5 g/10min

Show Supplier Material materials with Velocidad de flujo de la masa derretida of 4.5 g/10min

ASTM D1238, 190°C/2.16kg

Technological properties

Property
Application areas

Due to its combination of mechanical properties, ESCR resistance and fluidity, GREENETHENE G-3645UV is suggested for the production of wide variety of Storage tank applications of water, chemicals & Oils. GREENETHENE G-3645UV can also be used for off-shore flotation buoys and road crash barriers.

Certifications

List of Constituents of Polyethylene in Contact with Foodstuffs, Pharmaceuticals and Drinking Water: IS 10141:2001, IS 12701:1996

Color

Natural, black, terracotta, fire red, yellow and blue.

Processing methods

Compression molded & rotomolded