Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Conductividad térmica | 23.0 °C | 40 W/(m·K) Show Material materials with Conductividad térmica of 40 W/(m·K) | Typical for Tin Antimony |
Temperatura de fusión | 215 - 350 °C Show Material materials with Temperatura de fusión of 215 - 350 °C | Typical for Tin Antimony |
Chemical properties
Property | Value |
---|---|
Antimonio | 3 - 6 % Show Material materials with Antimonio of 3 - 6 % |
Bismuto | 0.5 % Show Material materials with Bismuto of 0.5 % |
Cadmio | 0.05 % Show Material materials with Cadmio of 0.05 % |
Cobre | 0.05 % Show Material materials with Cobre of 0.05 % |
Estaño | 94 % Show Material materials with Estaño of 94 % |
Plata | 0.05 % Show Material materials with Plata of 0.05 % |
Plomo | 0.25 % Show Material materials with Plomo of 0.25 % |