General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 9.6 g/cm³ Show Material materials with Densidad of 9.6 g/cm³ | Typical for Lead Antimony |
Mecánica
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 130 - 159 J/(kg·K) Show Material materials with Calor específico of 130 - 159 J/(kg·K) | Typical for Lead Antimony |
Conductividad térmica | 23.0 °C | 24 - 34 W/(m·K) Show Material materials with Conductividad térmica of 24 - 34 W/(m·K) | Typical for Lead Antimony |
Temperatura de fusión | 235 - 305 °C Show Material materials with Temperatura de fusión of 235 - 305 °C | Typical for Lead Antimony |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.01 % Show Material materials with Aluminio of 0.01 % |
Antimonio | 16 - 18 % Show Material materials with Antimonio of 16 - 18 % |
Arsénico | 0.08 % Show Material materials with Arsénico of 0.08 % |
Cobre | 2.5 - 3.5 % Show Material materials with Cobre of 2.5 - 3.5 % |
Estaño | 79 - 81 % Show Material materials with Estaño of 79 - 81 % |
Hierro | 0.08 % Show Material materials with Hierro of 0.08 % |
Plomo | 1.5 % Show Material materials with Plomo of 1.5 % |
Zinc | 0.01 % Show Material materials with Zinc of 0.01 % |