General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 12.7 g/cm³ Show Material materials with Densidad of 12.7 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Rockwell B | 20.0 °C | 77 - 90 [-] Show Material materials with Dureza Rockwell B of 77 - 90 [-] |
Resistencia a la flexión | 20.0 °C | 758 - 827 MPa Show Material materials with Resistencia a la flexión of 758 - 827 MPa |
Resistencia a la tracción | 20.0 °C | 379 - 448 MPa Show Material materials with Resistencia a la tracción of 379 - 448 MPa |
Eléctrico
Property | Value |
---|---|
Specific Electrical conductivity | 34 - 57 % IACS Show Material materials with Specific Electrical conductivity of 34 - 57 % IACS |
Chemical properties
Property | Value |
---|---|
Cobre | 38 - 42 % Show Material materials with Cobre of 38 - 42 % |