General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 13.7 g/cm³ Show Material materials with Densidad of 13.7 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Rockwell B | 20.0 °C | 85 - 98 [-] Show Material materials with Dureza Rockwell B of 85 - 98 [-] |
Resistencia a la flexión | 20.0 °C | 896 - 965 MPa Show Material materials with Resistencia a la flexión of 896 - 965 MPa |
Resistencia a la tracción | 20.0 °C | 516 - 585 MPa Show Material materials with Resistencia a la tracción of 516 - 585 MPa |
Eléctrico
Property | Value |
---|---|
Specific Electrical conductivity | 29 - 52 % IACS Show Material materials with Specific Electrical conductivity of 29 - 52 % IACS |
Chemical properties
Property | Value |
---|---|
Cobre | 28 - 32 % Show Material materials with Cobre of 28 - 32 % |