General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 14.3 g/cm³ Show Material materials with Densidad of 14.3 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Rockwell B | 20.0 °C | 89 - 102 [-] Show Material materials with Dureza Rockwell B of 89 - 102 [-] |
Resistencia a la flexión | 20.0 °C | 965 - 1034 MPa Show Material materials with Resistencia a la flexión of 965 - 1034 MPa |
Resistencia a la tracción | 20.0 °C | 585 - 654 MPa Show Material materials with Resistencia a la tracción of 585 - 654 MPa |
Eléctrico
Property | Value |
---|---|
Specific Electrical conductivity | 27 - 48 % IACS Show Material materials with Specific Electrical conductivity of 27 - 48 % IACS |
Chemical properties
Property | Value |
---|---|
Cobre | 23 - 27 % Show Material materials with Cobre of 23 - 27 % |