General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 15 g/cm³ Show Material materials with Densidad of 15 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Rockwell B | 20.0 °C | 94 - 106 [-] Show Material materials with Dureza Rockwell B of 94 - 106 [-] |
Resistencia a la flexión | 20.0 °C | 1034 - 1103 MPa Show Material materials with Resistencia a la flexión of 1034 - 1103 MPa |
Resistencia a la tracción | 20.0 °C | 620 - 689 MPa Show Material materials with Resistencia a la tracción of 620 - 689 MPa |
Eléctrico
Property | Value |
---|---|
Specific Electrical conductivity | 25 - 45 % IACS Show Material materials with Specific Electrical conductivity of 25 - 45 % IACS |
Chemical properties
Property | Value |
---|---|
Cobre | 18 - 22 % Show Material materials with Cobre of 18 - 22 % |