General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 16.4 g/cm³ Show Material materials with Densidad of 16.4 g/cm³ | Typical for Tantalum |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.34 [-] Show Material materials with Coeficiente de Poisson of 0.34 [-] | Typical for Tantalum |
Elongación | 20.0 °C | 10 - 20 % Show Material materials with Elongación of 10 - 20 % | |
Elongation A25 | 20.0 °C | 25 % Show Material materials with Elongation A25 of 25 % | |
Límite elástico Rp 0,2 | 20.0 °C | 103 MPa Show Material materials with Límite elástico Rp 0,2 of 103 MPa | |
Módulo de cizallamiento | 23.0 °C | 69 GPa Show Material materials with Módulo de cizallamiento of 69 GPa | Typical for Tantalum |
Módulo elástico | 23.0 °C | 185 GPa Show Material materials with Módulo elástico of 185 GPa | Typical for Tantalum |
Resistencia a la tracción | 20.0 °C | 244 MPa Show Material materials with Resistencia a la tracción of 244 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 147 J/(kg·K) Show Material materials with Calor específico of 147 J/(kg·K) | Typical for Tantalum |
Coeficiente de dilatación térmica | 23.0 °C | 6.5E-6 1/K Show Material materials with Coeficiente de dilatación térmica of 6.5E-6 1/K | Typical for Tantalum |
Conductividad térmica | 23.0 °C | 52 - 57 W/(m·K) Show Material materials with Conductividad térmica of 52 - 57 W/(m·K) | Typical for Tantalum |
Temperatura de fusión | 2996 °C Show Material materials with Temperatura de fusión of 2996 °C | Typical for Tantalum |
Chemical properties
Property | Value |
---|---|
Carbono | 0.01 % Show Material materials with Carbono of 0.01 % |
Hidrógeno | 1.5E-3 % Show Material materials with Hidrógeno of 1.5E-3 % |
Hierro | 0.01 % Show Material materials with Hierro of 0.01 % |
Molibdeno | 0.02 % Show Material materials with Molibdeno of 0.02 % |
Niobio | 35 - 42 % Show Material materials with Niobio of 35 - 42 % |
Nitrógeno | 0.01 % Show Material materials with Nitrógeno of 0.01 % |
Níquel | 0.01 % Show Material materials with Níquel of 0.01 % |
Oxígeno | 0.02 % Show Material materials with Oxígeno of 0.02 % |
Silicona | 5E-3 % Show Material materials with Silicona of 5E-3 % |
Titanio | 0.01 % Show Material materials with Titanio of 0.01 % |
Wolframio | 0.05 % Show Material materials with Wolframio of 0.05 % |